摘要
Inthiswork,compressive,flexuralandsplittensilestrengthtogetherwithcoefficientofwaterabsorptionofhighperformanceself-compactingconcretecontainingdifferentamountofFe2O3nanoparticleshavebeeninvestigated.ThestrengthandthewaterpermeabilityofthespecimenshavebeenimprovedbyaddingFe2O3nanoparticlesinthecementpasteupto4.0wt%.Fe2O3nanoparticleasaforeignnucleationsitecouldaccelerateC-S-HgelformationasaresultofincreasedcrystallineCa(OH)2amountespeciallyattheearlyageofhydrationandhenceincreasethestrengthofthespecimens.Inaddition,Fe2O3nanoparticlesareabletoactasnanofillersandrecovertheporestructureofthespecimensbydecreasingharmfulporestoimprovethewaterpermeability.Severalempiricalrelationshavebeenpresentedtopredicttheflexuralandthesplittensilestrengthofthespecimensbymeansofthecorrespondingcompressivestrengthatacertainageofcuring.Acceleratedpeakappearanceinconductioncalorimetrytests,moreweightlossinthermogravimetricanalysisandmorerapidappearanceofpeaksrelatedtohydratedproductsinX-raydiffractionresultsindicatethatFe2O3nanoparticlesupto4wt%couldimprovethemechanicalandthephysicalpropertiesofthespecimens.
出版日期
2012年01月11日(中国期刊网平台首次上网日期,不代表论文的发表时间)